Ceramic Foundry sand ,also called as Fused Ceramic Sand is made from high quality bauxite, by re-fused and blown to ball type. With advantage of fine surface smooth finish and air permeability, it is a new type casting material for precision casting, coated sand and self hardening sand etc.At the present, Ceramsite is acknowledged in the worldwide as the newest and the best ideal sand for the foundries and has a very wide feasibility of applications for the future development.
Chemical and Physical Composition:
Chemical Analysis[%] | |
Al2O3 | 70-75 |
SiO2 | 8-20 |
Fe2O3 | ≤3 |
TiO2 | ≤3.5 |
CaO | ≤0.45 |
MgO | ≤0.35 |
K2O | ≤0.33 |
Na2O | ≤0.08 |
Physical Properties | |
Grain shape | Spherical Ball |
Roundness | 90% |
Refractoriness: | >1790℃ |
Shape Coefficient | ≤1.1 |
Thermal Expansion Ratio | 0.13%(Heated up for 10 min at 1000℃) |
Thermal expansion coefficient | 6×10-6 /℃(20-1000℃) |
Thermal conductivity | 0.698W/M.K(1200℃) |
Specific Gravity:: | 1.95-2.05g/cm3 |
Bulk density(LPD): | 3.4 g/cm3 |
Color: | Black |
AVAILABLE SIZES | |
AFS25-35,AFS35-45,AFS45-55,AFS55-65,AFS60-70,AFS70-80,AFS95-110 Customized sizes are available upon request |
Products Show:
Application and how to choose available size:
1. Shell molding
2. Precision Casting
3. Lost foam casting
4. Heavy steel casting
5. Resin coated sand casting
6. Vacuum casting
7. Investment casting
Applications | Grit Size | AFS SIZE |
Foundry sand for Lost foam | 8-15#(10#)10-20#,20-30# | AFS25-35 |
Filler sand | 30# | |
No bake sand including furan resin /alkaline-phenolic resin molding and core making/ Pep set /Sodium-silicate bonded sand | 30-50#,40-70#,50-70#,70-140# | AFS35-45,AFS25-35,AFS45-55, AFS55-65,AFS60-70,AFS70-80 |
Shell molding, resin coated sand casting | 50-100#,70-140#,100-200# | AFS55-65,AFS60-70,AFS70-80, AFS95-110 |
Lost foam casting coating | 140-270#,-200# | |
Molding sand alcohol-based coating | -200# | |
3D printing, precision casting, investment casting | -140# |
Package(1TON JUMPO BAGS):